Sale
Zoom the image with mouse

Angelus Silano - Adhesion Promoter For Ceramics & Glass Fibers

Angelus
5ml Bottle
Rs. 1,150 Rs. 1,200
Pre activated (ready to use) adhesion promoter for ceramics and glass fibers
Key Features
1. Pre activated
2. Solvent based on ethanol
3. Better adhesion

Silano - Pre activated (ready to use) adhesion promoter for ceramics and glass fibers

  • In metal-free dentistry, an adhesive technique is fundamental for the cementation of all-ceramic, indirect composite resin restorations and glass fiber posts.
  • Adhesion of resin cements to enamel and dentin through acid-etching and application of priming and bonding agents are well known and researched  

How do resin cement bond with Composite/Fiber

  • Can bonding to cured composite resin be enhanced? The solution is in silanization.
  • Silanes are adhesion promoters between organic and inorganic materials. As bi-functional molecules, their silica radicals unite with the silica in the restorative materials and their organic radicals co-polymerize with the organic matrix of the resin.
  • Silanes are also called ceramic primers or bonding/coupling agents act as adhesion promoter for porcelain (ceramic) and glass fiber.

BENEFITS

  • Increases wettability of restorative materials in relation to resin cements, enhancing mechanical, physical and chemical adhesion between cement and restoration;
  • Increases resistance to dissolution by water at the cement-restoration interface.
  • Easy to use
  • Less evaporation
  • Enhances bonding of resin materials (resin and cements) to porcelain (ceramic) and glass fiber
  • Solvent based on ethanol: less evaporation
1. Treatment of internal surfaces of porcelain restorations and glass fiber posts before cementation with resin cements.
2. Treatment of porcelain surfaces before repair with composite resin.
3. Treatment of porcelain surfaces before bonding of porcelain.
Silane coupling agent
Instructions:

• CEMENTATION OF GLASS FIBER POSTS

1. Clean post with alcohol; dry with air;
2. Apply SILANO ANGELUS® with disposable applicators (APLIK ANGELUS®); wait for 1 (one) minute and gently dry with air
3. Proceed with cementation following instructions of the adhesive FUSION-DURALINK® ANGELUS® and of the selected resin cement

• CEMENTATION OF CERAMIC AND FIBER REINFORCED INDIRECT COMPOSITE RESIN RESTORATIONS

1. Isolate the margins of the restoration with wax to avoid marginal degradation by the hydrofluoric acid and adhesion of resin cement to the outer surface of the restoration
2. Apply PORCELAIN CONDITIONING agent (ANGELUS® - 10% Hydrofluoric Acid) on the internal area of the restoration; wait for 1 (one) minute* Leucite-based porcelains are etched only for 20 (twenty) seconds.
3. Wash with water and dry with air;
4. Apply SILANO ANGELUS® with diposable applicators (APLIK ANGELUS®); wait for 1 (one) minute and gently dry with air.
5. Proceed with cementation following instructions of the adhesive FUSION-DURALINK® ANGELUS® and of the selected resin cement.

• REPAIR OF CERAMIC AND INDIRECT COMPOSITE RESIN WITH DIRECT COMPOSITE RESIN

1. Bevel the fractured ceramic surface and roughen the metal (if exposed) or apply a layer of a metal primer (MZ PRIMER ANGELUS®)
2. Apply PORCELAIN CONDITIONING ANGELUS® (10% Hydrofluoric Acid) on the beveled surface and on the fracture site; wait for 1 (one) minute*, wash abundantly with water and dry Leucite-based porcelains are etched only for 20 (twenty) seconds.Protect oral tissues against the corrosive and poisonous effects of HF.
3. Apply SILANO ANGELUS® with a brush; wait for 1 (one) minute and gently dry with air
4. Apply the adhesive FUSION-DURALINK® ANGELUS® bonding agent following its instructions;
5. If there is exposed metal, cover it with a layer of OPAK ANGELUS® masking resin
6. Restore the fracture site with composite resin

• BONDING FRAGMENT OF CERAMIC OR INDIRECT COMPOSITE RESIN

1. Roughen fragment and fracture site;
2. Apply PORCELAIN CONDITIONING ANGELUS® (10% Hydrofluoric Acid) on fracture site and on fragment for 1 (one) minute*; wash and dry Leucite-based porcelains are etched only for 20(twenty) seconds.
3. Apply SILANO ANGELUS® with diposable applicators (APLIK ANGELUS®); wait for 1 (one) minute and gently dry with air ;
4. Cement fragment on restoration following instructions of the adhesive FUSION-DURALINK® ANGELUS® and of selected resin cement.

Storage:
Store at dry place

Customer Reviews

No reviews yet
0%
(0)
0%
(0)
0%
(0)
0%
(0)
0%
(0)
Angelus Silano - Adhesion Promoter For Ceramics & Glass Fibers
You have successfully subscribed!
This email has been registered
ico-collapse
0
Recently Viewed
Top
ic-expand
ic-cross-line-top